Hello! I’ve never had experience with SLA 3D printing, but I’m looking to try it now for prototyping purposes in the electronics/med-tech industry. I’ve heard that parts can become brittle over time due to UV light exposure. How does prolonged exposure to UV light (sunlight) specifically affect the brittleness and mechanical properties of SLA 3D prints made from ABS-like and PC-like resins? Would love to hear any practical experiences or insights on this. Thank you!

Solved by Nikolaus Mroncz
Hi Stefan, for prototypes, SLA still is fine. I would say, you can observe an aging and a change in proberties (by  getting brittle) after a couple of month. I don't see big differences between the standard resins here. To prevent this, you can , for example, spray paint the parts. Also SLS/ MJF combined with vapour smoothing could be an option. BR
    • S

      Hello! I’ve never had experience with SLA 3D printing, but I’m looking to try it now for prototyping purposes in the electronics/med-tech industry. I’ve heard that parts can become brittle over time due to UV light exposure. How does prolonged exposure to UV light (sunlight) specifically affect the brittleness and mechanical properties of SLA 3D prints made from ABS-like and PC-like resins? Would love to hear any practical experiences or insights on this. Thank you!

      0
    • Xometry Engineer

      Hi Stefan,

      for prototypes, SLA still is fine. I would say, you can observe an aging and a change in proberties (by  getting brittle) after a couple of month. I don’t see big differences between the standard resins here. To prevent this, you can , for example, spray paint the parts. Also SLS/ MJF combined with vapour smoothing could be an option.

      BR

      0
      Reply
      • S
        Nikolaus Mroncz

        Thank you, Nikolaus!

        I see that Xometry offers “quick clear coating” for Industrial Transparent, ABS-like material for SLA. Could this be an effective finish to mitigate UV light’s impact on the properties of the parts? If yes, can you please share how effective it is?

        0
        Reply
    • Xometry Engineer

      Quick Clear Coating is a spray painting with clear spray. It prevents the parts from the SLA typical yellowish and also to get fast brittle. It is very effective!

      0
      Reply
      • S
        Nikolaus Mroncz

        Thank you!

        0
        Reply
UV exposure impact on brittleness of SLA 3D parts
Your information:




Suggested Topics

Topic
Replies
Views
Activity
Choosing the right tool steel grade for a high-volume stamping die
hi, I’m designing a cold-formed stamping die for thin stainless-steel sheets (gauge ~1.5 mm) used in an enclosure that will see around 500 k cycles. Given that abrasion resistance and dimensional stability over long... read more
J
0
46
Dec 08
Blasting and anodizing order on aluminum parts
Hello! need help - am working on a set of 6061-T6 aluminum control knobs for a small instrument panel, and the surface finish is important since they’ll be handled frequently and remain visible. The... read more
J
C
1
194
Dec 09
Gasket material for short-term hydrotest on carbon steel piping
Looking for advice on selecting a gasket material for temporary spool joints during a hydrotest on carbon steel piping in a refinery. The test medium will be demineralized water (low conductivity, no additives), and... read more
C
N
1
153
Dec 08
Acrylic or pc for outdoor enclosures
hi! For transparent cover for an outdoor sensor needs to stay clear, handle some impacts, and resist sunlight - would you go with acrylic or polycarbonate? Acrylic has better UV and scratch resistance, but... read more
L
D
3
258
Nov 26