Passivation of stainless steel for harsh environment

0
F
2

Hello!

I’m working on a part that will be used in a harsh environment, so I was thinking of stainless steel 304 as a suitable material. I also would like to add a passivation finish to improve the corrosion resistance of the part.

Are there standardized grades or methods of passivation for stainless steel? What “grade” or specific type of passivation should I specify on the engineering drawing to ensure optimal corrosion resistance? There’s lots of info out there, but I’m a bit confused. Can anyone offer some straightforward guidelines?

Thanks in advance.

Solved by Joao Clemencio

Hello FSharaf,

There are indeed several standards and types of passivation.

The main standard grades you have available are: ASTM A967, AMS 2700 and ISO 16048.

In order to have a to ensure optimal corrosion I would specify "Passivate per ASTM A967, Citric Acid Method" on your engineering drawing.

ASTM A967: This standard covers the chemical passivation treatments for stainless steel, ensuring the part meets industry standards.
Citric Acid Passivation: It's environmentally safer and effective for stainless steel 304.

    • F

      Hello!

      I’m working on a part that will be used in a harsh environment, so I was thinking of stainless steel 304 as a suitable material. I also would like to add a passivation finish to improve the corrosion resistance of the part.

      Are there standardized grades or methods of passivation for stainless steel? What “grade” or specific type of passivation should I specify on the engineering drawing to ensure optimal corrosion resistance? There’s lots of info out there, but I’m a bit confused. Can anyone offer some straightforward guidelines?

      Thanks in advance.

      0
    • Xometry Engineer

      Hello FSharaf,

      There are indeed several standards and types of passivation.

      The main standard grades you have available are: ASTM A967, AMS 2700 and ISO 16048.

      In order to have a to ensure optimal corrosion I would specify “Passivate per ASTM A967, Citric Acid Method” on your engineering drawing.

      ASTM A967: This standard covers the chemical passivation treatments for stainless steel, ensuring the part meets industry standards.
      Citric Acid Passivation: It’s environmentally safer and effective for stainless steel 304.

      0
      Reply
      • F
        Joao Clemencio

        Hello Joao,

        Thanks for the info. I’ll specify this on the drawing, appreciate your help!

        0
        Reply
Passivation of stainless steel for harsh environment
Your information:




Suggested Topics

Topic
Replies
Views
Activity
Effect of zinc flake coating thickness on bolt performance
In an automotive subframe project using M12 class 10.9 bolts, exposed to salt spray and vibration, I’m looking into zinc flake coatings for corrosion protection. Curious if doubling the coating thickness—from 8 µm to... read more
B
0
4
Jun 20
direct metal laser sintering
I need to obtain hole/channel sizes of 0.65 mm. will this be obtainable with a 40-60 layer thickness in tool steel?
j
1
37
Jun 13
SLA material for outdoor indicator lenses
hi,  I'm recreating two small indicator lenses for a 1980s motorcycle restoration. These need to be clear, UV-stable, and able to handle exposure to sun and rain long-term. I’m planning to go with SLA... read more
R
V
1
122
May 08
Steel Advice
HelloI would like to request a quote for cold cutting tools (no temperature problems). I usually work with high-speed steels, for their hardness and the relative ease of re-sharpening, but none is offered in... read more
m
P
1
125
Apr 30
Fuel-resistant material for 3D printing
Hi! I'm restoring an older two-stroke motorcycle and need to replace a worn-out venturi nozzle that draws in fuel-air mix. I’m considering having it 3D printed, but I’m unsure which material would best hold... read more
A
M
1
137
May 02