Hi community, I’m working on injection-molded parts that need to have a consistent color across multiple production runs. The target color is pretty specific, so I’m trying to figure out the best way to communicate it for accuracy. I’ve come across the RAL and Lab* color systems but I’m not sure which one is best. Is providing a RAL code usually good enough, or is it worth using Lab* values to avoid color inconsistencies? Is it more reliable?

Solved by Danny94

In my experience, using Lab* values is the way to go if you need really tight color consistency, especially for larger production runs. RAL is great for general color matching, but it can have some variations depending on the manufacturer or the surface finish of your part. Lab* helps take that guesswork out since it’s more precise in how it defines color.

    • M

      Hi community, I’m working on injection-molded parts that need to have a consistent color across multiple production runs. The target color is pretty specific, so I’m trying to figure out the best way to communicate it for accuracy. I’ve come across the RAL and Lab* color systems but I’m not sure which one is best. Is providing a RAL code usually good enough, or is it worth using Lab* values to avoid color inconsistencies? Is it more reliable?

      0
    • D

      In my experience, using Lab* values is the way to go if you need really tight color consistency, especially for larger production runs. RAL is great for general color matching, but it can have some variations depending on the manufacturer or the surface finish of your part. Lab* helps take that guesswork out since it’s more precise in how it defines color.

      0
      Reply
Accurate color matching in injection molding
Your information:




Cancel

Suggested Topics

Topic
Replies
Views
Activity
Printed aluminum parts in pressure applications
Hi! Questioning about prototyping a hydraulic valve housing (normally CNC’d in 6061) - considering aluminum 3D printing instead, mainly to speed up design iterations. The part would see ~150 bar during bench tests, with... read more
T
0
64
Sep 29
High-temperature chemical pump housing in PEEK, tips on avoiding warpage?
Hi everyone, I'm working on a small pump housing for a chemical metering application. The part will be injection molded in PEEK, exposed to roughly 180 °C fluid and aggressive solvents. It's a compact... read more
S
R
4
175
Sep 30
Issues with polyurethane bonded rollers under load
Hi! Currently working on a small batch of U-groove guide rollers for a linear transfer system, and I'm using a soft polyurethane tread (around 85A Shore) bonded to aluminum hubs. The supplier estimates each... read more
P
A
4
667
Aug 19
Best fixture setup for milling and drilling mid-size batches of aluminum brackets?
Hi, I've got a batch of aluminum brackets that need to be drilled and milled on all sides with high repeatability. Has anyone designed a modular fixture system for parts like this to reduce... read more
h
u
a
9
939
Aug 22
Vacuum casting for snap-fits
I’m planning to use vacuum casting to produce about 50 housing units with integrated snap-fit features for an electronics prototype. The parts need to survive multiple assembly/disassembly cycles during testing. I’ve seen mixed opinions... read more
J
A
j
9
1.0k
Aug 11