My 3D prints need to withstand temperatures up to 150 degrees. What material should I choose?

Solved by Nikolaus Mroncz
Here, the choice largely depends on what type of material (metal or plastic) your part needs to be made of. For plastic parts, I would recommend the following materials:
  • ULTEM 9085 and ULTEM 1010 for FDM
  • PA 12 for SLS or MJF
  • Heat-resistant ones like PC for SLA after thermal post-processing
  • CE 221 (Cyanate Ester) for Carbon DLS
For metal parts, the heat-resistant materials I would recommend for DMLS are:
  • Aluminium AlSi10Mg
  • Stainless steel 316L
  • Inconel 718
You can check out our dedicated article on heat-resistant materials for 3D printing and compare the properties of the materials.
    • My 3D prints need to withstand temperatures up to 150 degrees. What material should I choose?

      0
    • Xometry Engineer

      Here, the choice largely depends on what type of material (metal or plastic) your part needs to be made of.

      For plastic parts, I would recommend the following materials:

      • ULTEM 9085 and ULTEM 1010 for FDM
      • PA 12 for SLS or MJF
      • Heat-resistant ones like PC for SLA after thermal post-processing
      • CE 221 (Cyanate Ester) for Carbon DLS

      For metal parts, the heat-resistant materials I would recommend for DMLS are:

      • Aluminium AlSi10Mg
      • Stainless steel 316L
      • Inconel 718

      You can check out our dedicated article on heat-resistant materials for 3D printing and compare the properties of the materials.

      0
      Reply
Heat resistant 3D printing material
Your information:




Suggested Topics

Topic
Replies
Views
Activity
sizing holes in sheet metal to receive PEM inserts
Hello all,Xometry's own design guidelines state that when PEM self clinching thread inserts are desired, one should refer to the insert manufacturer's design guidelines.The datasheet for the insert I'm interested in calls for a... read more
n
f
2
32
Sep 16
DMLS AlSi10Mg – Surface Finish Optimization & Leak-Proofing Methods
Hi everyone, I’m working with DMLS (AlSi10Mg) and looking for advice on post-processing. What finishing methods do you recommend to achieve a smooth (non-grainy) surface, especially for functional parts? Also, what’s the best approach... read more
p
1
566
Mar 27
Choosing a production process for low-volume over-molded elastomer grip
Hi! Deciding between low-volume production options for a small elastomeric over-molded grip on a handheld power tool. The part has undercuts and thin ribs, and we need decent tear resistance, but only ~200–300 pcs/year.... read more
A
S
B
2
2.3k
Mar 06
Choosing PA12 vs PA12-CF for an SLS-printed automotive cam cover prototype
hey, I’m working on a three-piece cam/valve cover for a small automotive engine project, mainly a functional prototype that will see real under-hood temperatures, oil mist, and vibration, but not long-term production use. The... read more
h
l
1
804
Jan 22