hi, I’m designing a cold-formed stamping die for thin stainless-steel sheets (gauge ~1.5 mm) used in an enclosure that will see around 500 k cycles. Given that abrasion resistance and dimensional stability over long runs are critical, I’m debating between a high-wear cold-work steel like a “D-series” (e.g. D2) or a hot-work steel even though the process is at room temperature. Has anyone tried cold-work tool steel for similar stamping dies under repeated cycling this high, and how did the material hold up in terms of dimensional accuracy vs. wear?

    • J

      hi, I’m designing a cold-formed stamping die for thin stainless-steel sheets (gauge ~1.5 mm) used in an enclosure that will see around 500 k cycles. Given that abrasion resistance and dimensional stability over long runs are critical, I’m debating between a high-wear cold-work steel like a “D-series” (e.g. D2) or a hot-work steel even though the process is at room temperature. Has anyone tried cold-work tool steel for similar stamping dies under repeated cycling this high, and how did the material hold up in terms of dimensional accuracy vs. wear?

      0
    • D

      It sounds like D2 is exactly the right choice for your stamping die. It’s a high-chromium tool steel, so well-suited to being used with stainless. Also, since your process will be at room temperature, just use the “right” (cold-work) tool steel for that temperature. Regarding your concerns about wear over 500k cycles, there are some generalized performance results out of Germany that suggest the die may see wear rounding at about half that production run (250k cycles). However, I don’t think you’re going to get a better performing alloy; D2 is perfectly suited to this. I think you’re trying to get too fancy (to your own detriment) if you want to try to use a hot-work steel for this stamping.

      0
      Reply
Choosing the right tool steel grade for a high-volume stamping die
Your information:




Suggested Topics

Topic
Replies
Views
Activity
Contact
Good day, I have been trying to receive the materials I paid for, for several days now. It's impossible to speak with anyone who can provide a serious and reliable update. The service is... read more
c
0
36
Aug 25
3D Printing
Good morning, I would like a quote. I have attached some photos of 3D designs already created with AutoCAD as solids. I also have the DWG file that you can reference or use as... read more
l
1
42
Aug 20
Request for Material Information for Trumpet Mouthpiece
Good day. I have a trumpet mouthpiece that I have modeled myself using FreeCAD, which I need to print. I conducted a small research and Google suggests using PETG (Polyethylene Terephthalate Glycol-modified) as a... read more
m
2
94
Jul 29
DMLS AlSi10Mg – Surface Finish Optimization & Leak-Proofing Methods
Hi everyone, I’m working with DMLS (AlSi10Mg) and looking for advice on post-processing. What finishing methods do you recommend to achieve a smooth (non-grainy) surface, especially for functional parts? Also, what’s the best approach... read more
p
1
514
Mar 27