en – Global
Knowledge & Community
Search
K
Quote & source your parts
select
navigate
switch tabs
Esc close

MEI industry pieces

0
3

mei

Automatically translated from: Français
See original
Solved by Manon Bouriaud

Hello Benjamin,
Do you have a question to ask? It seems that your message has been truncated, and in its current state it is not very useful to the Community.

    • mei
      Automatically translated from: Français

      See original
      0
    • Senior Content Manager

      Hello Benjamin,
      Do you have a question to ask? It seems that your message has been truncated, and in its current state it is not very useful to the Community.

      Automatically translated from: Français

      See original
      0
      Reply
    • A glass plate and give it a shiny effect.

      Automatically translated from: Français

      See original
      0
      Reply
    • Perfect!

      Automatically translated from: Français

      See original
      0
      Reply
MEI industry pieces
Your information:




Suggested Topics

Topic
Replies
Views
Activity
DMLS AlSi10Mg – Surface Finish Optimization & Leak-Proofing Methods
Hi everyone, I’m working with DMLS (AlSi10Mg) and looking for advice on post-processing. What finishing methods do you recommend to achieve a smooth (non-grainy) surface, especially for functional parts? Also, what’s the best approach... read more
p
0
23
Mar 20
Choosing a production process for low-volume over-molded elastomer grip
Hi! Deciding between low-volume production options for a small elastomeric over-molded grip on a handheld power tool. The part has undercuts and thin ribs, and we need decent tear resistance, but only ~200–300 pcs/year.... read more
A
S
B
2
327
Mar 06
Choosing PA12 vs PA12-CF for an SLS-printed automotive cam cover prototype
hey, I’m working on a three-piece cam/valve cover for a small automotive engine project, mainly a functional prototype that will see real under-hood temperatures, oil mist, and vibration, but not long-term production use. The... read more
h
l
1
423
Jan 22
Surface Finish
I am looking to have some Aluminium samples made............without adding extra post process operations what is the best surface finish possible (um) ?
a
j
1
347
Jan 20
Choosing the right tool steel grade for a high-volume stamping die
hi, I’m designing a cold-formed stamping die for thin stainless-steel sheets (gauge ~1.5 mm) used in an enclosure that will see around 500 k cycles. Given that abrasion resistance and dimensional stability over long... read more
J
D
1
500
Dec 17