Vapor smoothed and dyed black part MJF vs. SLS

0
6

Hi there,
Can someone tell me how does the black dyed MJF nylon with vapor smoothing compare with black dyed SLS nylon with vapor smoothing? Specifically with regards to surface finish and visible layer lines.

Solved by Nikolaus Mroncz
Thanks for your questions! Here I share some images, how the parts may look: The first is SLS and the second MJF. Finally the parts may look quite similar, still it also depends on the design.
    • Hi there,
      Can someone tell me how does the black dyed MJF nylon with vapor smoothing compare with black dyed SLS nylon with vapor smoothing? Specifically with regards to surface finish and visible layer lines.

      0
    • Xometry Engineer

      Thanks for your questions!

      Here I share some images, how the parts may look:

      The first is SLS and the second MJF. Finally the parts may look quite similar, still it also depends on the design.

      0
      Reply
      • Nikolaus Mroncz

        Thanks Nikolaus for sharing these pictures! Indeed, the surface looks quite the same. What about the cost? Is it less expensive to apply such finishes on an MJF or SLS nylon part? 

        0
        Reply
    • Xometry Engineer

      For this, please try our Instant Quoting Engine. You can upload the part on our website and see immediately the price, also if you change the technology. It depends on volume and design of the part, so not to answer, the one or the other.

      0
      Reply
Vapor smoothed and dyed black part MJF vs. SLS
Your information:




Suggested Topics

Topic
Replies
Views
Activity
Teeth shearing off, what is the best material?
Hello, we have this small tool used to loosen/tighten a metal slotted ferrule. The teeth of the tool engage with the slots in the ends of the ferrule and torque is applied to tighten... read more
a
0
115
DMLS AlSi10Mg – Surface Finish Optimization & Leak-Proofing Methods
Hi everyone, I’m working with DMLS (AlSi10Mg) and looking for advice on post-processing. What finishing methods do you recommend to achieve a smooth (non-grainy) surface, especially for functional parts? Also, what’s the best approach... read more
p
1
485
Mar 27
Choosing a production process for low-volume over-molded elastomer grip
Hi! Deciding between low-volume production options for a small elastomeric over-molded grip on a handheld power tool. The part has undercuts and thin ribs, and we need decent tear resistance, but only ~200–300 pcs/year.... read more
A
S
B
2
1.5k
Mar 06
Choosing PA12 vs PA12-CF for an SLS-printed automotive cam cover prototype
hey, I’m working on a three-piece cam/valve cover for a small automotive engine project, mainly a functional prototype that will see real under-hood temperatures, oil mist, and vibration, but not long-term production use. The... read more
h
l
1
777
Jan 22