Hey , we’re looking for advice on achieving waterproof electronic card casings, since we’ve faced a few challenges lately. We’ve iterated several manufacturing processes: SLA, which resulted in warping due to thin walls, and MJF, where we removed the ESD constraint but still encountered issues with water ingress through porosity. A topical spray was tried to seal the MJF part, but the result was uneven, with a slightly sticky surface. Can anyone recommend a material or finish that would provide effective waterproofing while maintaining lightweight and cost-efficiency? We’d prefer to stick with additive methods for design flexibility and lower production volumes.

Solved by R Petersen
This is a pretty typical issue when producing waterproof housings for electronics. Via additive manufacturing, mitigating porosity in MJF is quite effective by vacuum impregnation. After printing, the part is immersed in a resin in a vacuum chamber, filling microvoids and curing in place a watertight seal. It’s reliable and maintains the lightweightness of the structure. You could CVD/PVD coat, providing a uniform, durable layer, but these tend to be really expensive, with complex setups. The penetration level can also be quite variable. Vacuum impregnation is way easier, especially for smaller production runs.
    • M

      Hey , we’re looking for advice on achieving waterproof electronic card casings, since we’ve faced a few challenges lately. We’ve iterated several manufacturing processes: SLA, which resulted in warping due to thin walls, and MJF, where we removed the ESD constraint but still encountered issues with water ingress through porosity. A topical spray was tried to seal the MJF part, but the result was uneven, with a slightly sticky surface. Can anyone recommend a material or finish that would provide effective waterproofing while maintaining lightweight and cost-efficiency? We’d prefer to stick with additive methods for design flexibility and lower production volumes.

      0
    • R

      This is a pretty typical issue when producing waterproof housings for electronics. Via additive manufacturing, mitigating porosity in MJF is quite effective by vacuum impregnation. After printing, the part is immersed in a resin in a vacuum chamber, filling microvoids and curing in place a watertight seal. It’s reliable and maintains the lightweightness of the structure.

      You could CVD/PVD coat, providing a uniform, durable layer, but these tend to be really expensive, with complex setups. The penetration level can also be quite variable. Vacuum impregnation is way easier, especially for smaller production runs.

      0
      Reply
      • M
        R Petersen

        Got it. Are there materials that naturally resist water ingress better than nylon?

        0
        Reply
      • R
        Misha Campbell

        Nylons can be good – depends on which one. PEEK or Nylon12 with additives can reduce porosity and improve surface voids. Also, SLA can work if you opt for engineering rather than general-grade resins. Those specified for dental or industrial applications minimize warping and are easier to post-process for waterproofing.

        0
        Reply
Best process to 3D print electronic card casing
Your information:




Suggested Topics

Topic
Replies
Views
Activity
sizing holes in sheet metal to receive PEM inserts
Hello all,Xometry's own design guidelines state that when PEM self clinching thread inserts are desired, one should refer to the insert manufacturer's design guidelines.The datasheet for the insert I'm interested in calls for a... read more
n
f
2
34
Sep 16
DMLS AlSi10Mg – Surface Finish Optimization & Leak-Proofing Methods
Hi everyone, I’m working with DMLS (AlSi10Mg) and looking for advice on post-processing. What finishing methods do you recommend to achieve a smooth (non-grainy) surface, especially for functional parts? Also, what’s the best approach... read more
p
1
570
Mar 27
Choosing a production process for low-volume over-molded elastomer grip
Hi! Deciding between low-volume production options for a small elastomeric over-molded grip on a handheld power tool. The part has undercuts and thin ribs, and we need decent tear resistance, but only ~200–300 pcs/year.... read more
A
S
B
2
2.3k
Mar 06
Choosing PA12 vs PA12-CF for an SLS-printed automotive cam cover prototype
hey, I’m working on a three-piece cam/valve cover for a small automotive engine project, mainly a functional prototype that will see real under-hood temperatures, oil mist, and vibration, but not long-term production use. The... read more